Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styrolution® PS 165N - PS - INEOS Styrolution

Material Data Center offers the following functions for Styrolution® PS 165N:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Styrolution PS datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Styrolution® PS 165N is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 3.4 cm³/10min ISO 1133
Temperatura 200 °C -
Carico 5 kg -
Densità del fuso 936 kg/m³ -
Conduttività termica del fuso 0.155 W/(m K) -
Capacità termica specifica del fuso 2300 J/(kg K) -
Temperatura di estrazione 82 °C -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3300 MPa ISO 527
Carico unitario a rottura 52 MPa ISO 527
Deformazione a rottura 2 % ISO 527
Modulo di scorrimento a trazione, 1h 3300 MPa ISO 899-1
Modulo di scorrimento a trazione, 1000h 2600 MPa ISO 899-1
Resistenzia all'urto Charpy con intaglio, +23°C 3 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di transizione vetrosa, 10°C/min 90 °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 76 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 84 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 89 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 80 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.5 mm -
Yellow Card disponibile - -
Reazione al fuoco a spessore h HB class IEC 60695-11-10
Spessore provato 3.2 mm -
Yellow Card disponibile - -
Indice di ossigeno 18 % ISO 4589-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 2.5 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 2.5 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 0.9 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 0.7 E-4 IEC 62631-2-1
Res. Alle correnti striscianti superficiali 375 - IEC 60112
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1040 kg/m³ ISO 1183
Proprietà Specifiche MaterialeValoreUnitáNorma del test
ISO Data
Numero di viscosità 119 cm³/g ISO 307, 1157, 1628
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 230 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 40 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Funzioni
Viscosità-Velocità di taglio , Styrolution® PS 165N, PS, INEOS Styrolution
Sforzo di taglio-Velocità di taglio , Styrolution® PS 165N, PS, INEOS Styrolution
Sforzi-deformazione , Styrolution® PS 165N, PS, INEOS Styrolution
Modulo secante-deformazione , Styrolution® PS 165N, PS, INEOS Styrolution
Sforzi-deformazioni (isocrona) 23°C, Styrolution® PS 165N, PS, INEOS Styrolution
Modulo di scorrimento-tempo 23°C, Styrolution® PS 165N, PS, INEOS Styrolution
Curva di scorrimento 23°C, Styrolution® PS 165N, PS, INEOS Styrolution
Volume specifico-temperatura (pvT) , Styrolution® PS 165N, PS, INEOS Styrolution
Modulo a taglio-temperatura , Styrolution® PS 165N, PS, INEOS Styrolution
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Film, Estrusione Profilati, Estrusione di Lastre/Fogli, Altre Estrusioni
Forma fisica disponibile
Pellet
Caratteristiche speciali
Trasparente
Disponibilità geografica
Europa, Near East/Africa
Altre informazioni
Stampaggio ad Iniezione
PROCESSING
injection molding, Melt temperature, range: 180 - 280 °C
injection molding, Melt temperature, recommended: 230 °C
injection molding, Mold temperature, range: 10 - 60 °C
injection molding, Mold temperature, recommended: 40 °C

Polystyrol 165N can be injection molded at temperatures between 180 and 280°C.Recommended mold temperatures are between 10 and 60°C.
Estrusione Film
PROCESSING
Extrusion, Blown film, Melt temperature: 180 - 210 °C
Extrusion, Flat film, Melt temperature: 200 - 240 °C

Extrusion melt temperature should not exceed 240°C.
Altre Estrusioni
PROCESSING
Extrusion, Pipes, Melt temperature: 180 - 210 °C
Estrusione di Profilati
PROCESSING
Extrusion, Profiles, Melt temperature: 210 °C
Estrusione Lastre/Fogli
PROCESSING
Extrusion, Plates, Melt temperature: 200 - 230 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com